RECYCLING PROCESS FOR TANTALUM AND SOME OTHER .
the air at 1150 K for 30 min, and the epoxy resin was oxidized (Fig. 2 (c)). The iron and nickel terminals were removed by magnetic separation, because these terminals were disconnected from the electrodes after oxidation (Fig. 2 (d)). After oxidation, the epoxy resin became a powder, which is chiefly consisted of SiO2. The sintered tantalum ...